Muggy Weld Silver Solder Starter Kit - 4 x 18" Rods

Be the first to review this product

$135.00
Use Your Points:
You will earn 135 Caswell Gold Rewards Points for buying this product
OR

Quick Overview

SKU: SSF-6
Muggy Weld Silver Solder Starter Kit - 4 x 18" Rods

Muggy Weld Silver Solder Starter Kit - 4 x 18" Rods

Double click on above image to view full picture

Zoom Out
Zoom In

More Views

Muggy Weld SSF-6 Silver Solder

Silver Solder on Steel Brass Copper Stainless Steel Using SSF-6 Silver Soldering Rod

  • Cadmium Free silver solder
  • Special "fast flow" flux coating provides twice the base metal cleansing action of conventional silver flux coatings
  • No odors from rubberized compounds yet the flux coating is totally flexible and non-fragile
  • The only flux coated silver solder strong enough to clean oxidized stainless steel
  • Ideal for food and pharmaceutical applications
  • Wets even burned stainless steel.
  • 1" of our high content silver solder will flow 18"--the only silver solder manufactured with this capability

Applications:

  • Steel, stainless steel, cast iron, copper, brass and bronze. Can be used on any combination of these metals.

Contains:

  • 4 x 18" flux coated rods 
TYPICAL MECHANICAL PROPERTIES

Undiluted Weld Metal

Maximum Value up to

Tensile Strength

71,000 PSI

Yield Strength

60,000 PSI

Elongation

25%

Conductivity

14.3

Density

9.59/cm3

Hardness

Brinell 130

Braze or Solder Steel to Stainless with High Strength Silver Solder