Black Magic Car Gas Tank Sealer

Be the first to review this product

$99.99
You will earn 99 Caswell Gold Rewards Points for buying this product
OR

Quick Overview

SKU: GTSCBM
Black Magic Car Gas Tank Sealer Kit

Black Magic Car Gas Tank Sealer

Double click on above image to view full picture

Zoom Out
Zoom In

More Views

Black Magic Gas Tank Sealer

Permanently Repairs Steel, Aluminum, Fiberglass and Plastic Gas Tanks

  • The same phenol novolac chemistry as our regular Gas Tank Sealer product.
  • Ethanol Resistant Chemistry. Withstands racing fuels and alcohol.
  • Black Color Makes For Easy Identification of Missed Areas
  • Each kit treats tanks up to 20 gallons

Application Instructions

All traces of oil and gasoline should first be removed by pouring about 1 pint of acetone or lacquer thinner into the tank, and rotating the tank several times to thoroughly sluice the sides with solvent. Dispose of the contaminated solution.

When recoating your gas tank from failed Kreem or POR-15 tank sealers, remove the old, failed coating using a paint stripper containing Methylene Chloride.

Place a hand full of drywall screws into the tank and shake them around vigorously for several minutes. These will dislodge any loose particles of rust. In the case of Fiberglass and plastic tanks, this will rough up the tank interior, improving adhesion.

Rinse out the tank with about 1-pint of acetone or lacquer thinner, then set aside and allow to dry. Use an airline to blow air into the tank to aid drying.

Apply duct tape or masking tape to any weeping seams, holes or porous areas. This will stop any Gas Tank Sealer from oozing out, and will allow it to bridge over the hole. Plug the outlet ports with putty or Play-Doh. Mix up the required amount of Gas Tank Sealer (one unit should treat two small motorcycle tanks or one large one) If you are only treating ONE small tank, then divide parts A & B in half. You could use a dipstick to gauge this.

In a separate plastic container (margarine tub etc.) mix the two parts together thoroughly for at least 2 minutes. Scrape around the sides to ensure all resin is blended together. BAD MIXING AND BAD MEASURING IS THE #1 CAUSE OF FAILURE!!

Pour into the tank, then immediately seal up the filler hole with Gladwrap and an elastic band. Swill the tank around in every direction for several minutes to obtain a good layer of Gas Tank Sealer over all surfaces. Remove the filler cap,Gladwrap seal, and pour out any excess. Allow to drain upside down for a few minutes.
If you have a built in fuel filter, blow air into the fuel line port for about 10 minutes. This will clear the filter of any Gas Tank Sealer.

Scrape off any excess with a sharp knife at this point (usually about 40-60 Min after mixing) Place the tank in a warm 70-90 f place and allow to cure overnight. In the case of alcohol fuels, allow 3-5 days at room temperature, or 24 hours at 120 deg f.