Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > Powder Coating Supplies > Liquiguard PC
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Liquiguard® PC

Liquiguard

Revolutionary Pre-Treatment For Powder Coating

Liquiguard®, an unprecedented water based non-hazardous, non-toxic coating developed for water proofing and rust and corrosion protection, now finds a unique application in the powder coating industry. Liquiguard’s anti-rust and bonding properties make it an excellent replacement for various phosphate pre-treatments.

Numerous benefits of Liquiguard pre-treatment are:

  1. Pre-treating with Liquiguard requires just two steps, cleaning and coating the part.
  2. Reduction in time used for pre-treatment results in better work flow and efficiency and savings.
  3. Large parts can be sprayed or brushed with Liquiguard.
  4. If rust spots are missed in the cleaning process, Liquiguard will isolate and inhibit rusting.
  5. Its non-toxic nature precludes the need for extraordinary measures in its use or disposal.
  6. Liquiguard has shown excellent tolerance in salt spray tests

Liquiguard® PC for Aluminum

Liquiguard® PC for Aluminum is specifically engineered to work best on aluminum grade products.
Liquiguard®PC Al is primarily used for aluminum, casting, magnesium, copper is proven to reduce out-gassing on aluminum substrates.

Applications Of This Product
  • Increase corrosion resistance of powder coated items.

Related Products

Liquiguard® PC is supplied ready to use and can be applied via dipping, spraying or brushing. A single base coat should be allowed to dry for 15 minutes or until tack free prior to powder coating. Depending on application method, each gallon provides approximately 750 square feet of base coat.

How To Use Liquiguard® PC

  1. Liquiguard PC is a water based, eco-friendly pre-treatment.
  2. Liquiguard PC should be stored in an ambient temperature above 55° F.
  3. Make sure the substrate is degreased, clean and dry.
  4. Liquiguard can be applied via spraying (HVLP, cup or gun fine mist nozzle) or dipping.
  5. Liquiguard PC is supplied ready to use. No diluting is required.
  6. It is essential to use a new or thoroughly clean nozzle which is free of all acids or contaminants and has a pH level of 7 or greater.
  7. Apply with an even spray that creates a light mist. Heavy spraying may cause the product to run.
  8. Make sure to cover all areas of the substrate.
  9. DO NOT RINSE.
  10. Let the substrate sit for 15-20 minutes or until tack-free, or place for five minutes in an oven between 375-400°.
  11. DO NOT RINSE.
  12. Now you are ready to powder coat as normal.
Quantity Product Code Name Size Price  
LGPC Liquiguard PC Primer 1 Gal $24.99
No Air Shipping
LGPCAL Liquiguard PC AL Primer 1 Gal $24.99
No Air Shipping
  - Order 5 Gallons & Save. Enter 5 in Quantity Fields Above 5 Gal $99.00
No Air Shipping
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
   
Login or Email
Password
Lost Password?
Create An Account