Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > Powder Coating Supplies > High Temp Ceramic Coatings
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

High Temp Ceramic Coatings

NOW AVAILABLE IN SMALLER SIZES

Black Eclipse Stoplight Red Screamin Yellow Blue Flame
Lollypop Purple Cerakote Gold    

Cerakote Exotic Color coatings are available in six unique colors.  These coatings were designed to withstand temperatures in excess of 800°F, while still maintaining their vibrant colors. Not only do these coatings offer excellent corrosion protection, but they retain an excellent appearance even after exposure to brake fluid, solvents, grease, oil, and extreme ultra-violet light.

These finishes are excellent for use on brake calipers, carburetors, intake manifolds, and other mid temperature applications. Available in four exotic colors, these finishes and properties are unique to the industry.

Air Cures in 24 hours. Products have a 6 month shelf life. 4oz will cover 50 sq ft at 1 mil thickness. Quart covers 400 sq ft at 1 mil thickness.

 

  • Black Eclipse C-141
  • Blue Flame C-158
  • Screamin' Yellow C-144
  • Stop Light Red C-143
  • Lollypop Purple C-163
  • Gold C-122
  • Chrome Available Here
Applications Of This Product

You Must Supply

Blasting Equipment

Spraygun

Vibratory Tumbler


Related Products

Preparation of substrate is crucial for maximum adhesion and performance of this material

  1. Remove all coatings, oils, and contaminates from substrate with either a de-greasing chemical and/or by heating substrate to temperatures high enough to remove coatings or contaminates.
  2. A blasted profile must be applied to the substrate to remove any rust, scale, or other coatings. This is required to ensure maximum adhesion. For best results use a dry grit material such as aluminum oxide or garnet equivalent to a 100 - 120 mesh size. Mask and plug all areas where coating is not desired. Remove any sharp edges or burrs that may create thin areas or protrude through coating.
  3. Place parts in an oven at 450°F for approximately 30 minutes to evaporate any last minute moisture, oils, or contaminates that blasting or contact with skin have deposited on surface. Do not apply any solvents to substrate after a blast profile has been applied.
  4. Hang parts to allow for best view and application access. Do not touch parts with bare skin.
  5. Make sure the “C” Series products are completely mixed and no solids remain in the bottom of the container. Failure to completely disperse the product will result in poor chemical ratios and product failure.
  6. Recommended spray equipment is a HVLP (gravity fed) spray gun. The use of a small spray tip pattern will aid in coating hard to reach areas without excessive build up in surrounding areas. Material does not need to be thinned. Use as received.
  7. Blow off substrate with a high-pressure air nozzle to remove any blasting dust left on the surface. Wear safety goggles or face shield for your protection.
  8. One applications of product is recommended for a 0.6 to 0.8 mil film thickness. Work from the most difficult surface out to the easiest. This will aid in reducing runs or excessive build up. NOTE: Always spray coating in a well ventilated area. Be aware of over-spray so it will not land on any item that is not to be coated.
  9. Parts will be tack free after approximately 35 minutes.
  10. Parts will be partially cured after 24 hours. Full cure and hardness does not take place until 5 to 6 days after application.
  11. Finished goods may be shipped after 24 hours.
  12. Clean tools and equipment with acetone or xylene.
Quantity Product Code Name Size Price  
NICC1414 Cerakote Black Eclipse 4 oz $37.99
No Air Shipping
NICC1418 Cerakote Black Eclipse 8 oz $69.99
No Air Shipping
NICC141P Cerakote Black Eclipse 16 oz $129.99
No Air Shipping
NICC141 Cerakote Black Eclipse 1 Quart $181.68
No Air Shipping
NICC1584 Cerakote Blue Flame 4 oz $34.99
No Air Shipping
NICC1588 Cerakote Blue Flame 8 oz $64.99
No Air Shipping
NICC158P Cerakote Blue Flame 16 oz $114.99
No Air Shipping
NICC158 Cerakote Blue Flame 1 Quart $199.99
No Air Shipping
NICC1444 Cerakote Screamin' Yellow 4 oz $39.99
No Air Shipping
NICC1448 Cerakote Screamin' Yellow 8 oz $74.99
No Air Shipping
NICC144P Cerakote Screamin' Yellow 16 oz $139.99
No Air Shipping
NICC144 Cerakote Screamin' Yellow 1 Quart $259.00
No Air Shipping
NICC1434 Cerakote Stop Light Red 4 oz $37.99
No Air Shipping
NICC1438 Cerakote Stop Light Red 8 oz $69.99
No Air Shipping
NICC143P Cerakote Stop Light Red 16 oz $129.99
No Air Shipping
NICC143 Cerakote Stop Light Red 1 Quart $181.68
No Air Shipping
NICC1224 Cerakote Gold 4 oz $29.99
No Air Shipping
NICC1228 Cerakote Gold 8 oz $56.99
No Air Shipping
NICC122P Cerakote Gold 16 oz $99.99
No Air Shipping
NICC122 Cerakote Gold 1 Quart $170.93
No Air Shipping
NICC1634 Cerakote Lollypop Purple 4 oz $39.99
No Air Shipping
NICC1638 Cerakote Lollypop Purple 8 oz $75.99
No Air Shipping
NICC163P Cerakote Lollypop Purple 16 oz $139.99
No Air Shipping
NICC163 Cerakote Lollypop Purple 1 Quart $200.00
No Air Shipping
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
  * - Other minor household items may be required, such as gloves, dust mask etc.
Login or Email
Password
Lost Password?
Create An Account