Pick A Buff Home
Polishing Iron & Steel
1st Stage - Rough Cut To Remove Scratches
Use
Sisal Wheel
With
Emery
(Black) Compound
2nd Stage - Final Cut and Initial Polish
Use
Spiral Sewn Wheel
With
Blizzard
(White) Compound
3rd Stage - Final Polish (or Luster)
Use
Loose Cotton Wheel
With
Blue Rouge
(Blue) Compound