Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
Login To Your Account
 
Home > Plating, Anodizing and Metal Finishing > MetalX Copper Stripper
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Ask Plating Questions On Our Forum

Online Plating Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

MetalX Copper Stripper

 

AN ELECTRICAL COPPER STRIPPER
FOR STRIPPING COPPER FROM STEEL OR
ALUMINUM

MetalX Copper Stripper is an electrical copper stripper with the exceptional ability to throw into very deep recesses. It also has the ability to plate out the stripped copper making the bath last indefinitely. It contains no ammonia or ammonia compounds.

Applications Of This Product
  • Strip copper from steel or aluminum.

Related Products

 

  • 2.5 lbs of Copper Stripper stripper makes 1 gallon of stripping solution.
  • Use plastic or lined stainless steel tanks. If unlined stainless steel tanks are used, some copper will stick to the tank walls.
  • Stripping tank can operate at room temperature. In cold climates, heat may be used to raise the tank temp to 80-120F. Use a titanium or glass heater.
  • Use Stainless Steel or copper cathodes.
  • Use steel or titanium wire to hang the parts. Copper wire will be dissolved.
  • A DC power source with an adjustable voltage of 0-12V is required. Amperage requirements are approximately 20 amps per square foot of part surface area. (0.13 amps per square inch)
  • Agitation should be used. Occasional filtration is recommended to remove small particles of copper from the bath.
  • To use, connect part to positive side of power supply. Connect cathodes to negative side. Stripping usually requires 3-6V DC.
  • Instruction sheet will be provided with purchase.

Copper Stripping Kit

The copper stripping kit contains everything you need, except a DC power supply, to strip copper from aluminum and steel.

1 Gallon Kit Contains:

  • 2 Gallon Tank and Lid
  • 2.5 lbs MetalX Copper Stripper (makes 1 gallon)
  • 2 x Stainless Steel Anodes
  • 1 x 300W Titanium Heater
  • 1 x Thermostat
  • 1 x 6' Titanium Wire
  • 1 x Filter Pump/Agitator
  • Instruction Sheet

2 Gallon Kit Contains:

  • 2.5 Gallon Tank and Lid
  • 5 lbs MetalX Copper Stripper (makes 2 gallons)
  • 2 x Stainless Steel Anodes
  • 1 x 300W Titanium Heater
  • 1 x Thermostat
  • 1 x 6' Titanium Wire
  • 1 x Filter Pump/Agitator
  • Instruction Sheet

 

Quantity Product Code Name Size Price  
METALXCU MetalX Copper Stripper (1 Gallon) 2.5 lb $35.00
Not Hazardous
  METALXCU MetalX Copper Stripper (2 Gallon) - Choose 2 From Quantity Field 5 lb $65.00
Not Hazardous
  METALXCU MetalX Copper Stripper (5 Gallon) - Choose 5 From Quantity Field 12.5 lb $145.00
Not Hazardous
  METALXCU MetalX Copper Stripper (10 Gallon) - Choose 10 From Quantity Field 25 lb $250.00
Not Hazardous
CSKIT1 Copper Stripping Kit 1 Gal $89.00
Not Hazardous
CSKIT2 Copper Stripping Kit 2 Gal $109.00
Not Hazardous
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
  * - Other minor household items may be required, such as gloves, water etc.