House Of Kolor Kosmic Kolors Reducers, Retarders & Catalysts |
|
|
|
FAST DRY REDUCER (RU310)
RU310 is recommended for use with our Kosmic Kolor® Base Coats, Shimrin® Base Coats, Kandys, and Klears. Has staged release for proper flow out, leveling, and gloss retention.
|
|
MEDIUM DRY REDUCER (RU311)
RU311 is recommended for use with our Kosmic Kolor® Base Coats, Shimrin® Base Coats, Kandys, and Klears. Has staged release for proper flow out, leveling, and gloss retention.
|
 |
SLOW DRY REDUCER (RU312)
RU312 is recommended for use with our Kosmic Kolor® Base Coats, Shimrin® Base Coats, Kandys, and Klears. Has staged release for proper flow out, leveling, and gloss retention.
|
|
 |
| The House Of Kolor Kosmic Kolor Urethane System offer the deepest, cleanest and richest colors in the industry. |
|
|
|
 |
VERY SLOW DRY REDUCER (RU313)
RU313 is recommended for use with our Kosmic Kolor® Base Coats, Shimrin® Base Coats, Kandys, and Klears. Has staged release for proper flow out, leveling, and gloss retention.
|
 |
VOC EXEMPT REDUCER (RU300)
RU300 can be used to reduce all Kosmic System products: Kandys, Clears, and all Shimrin ‚ base coat It will not change the VOC content of any product it is added to, and will not react with any coating. It is a fast to medium dry reducer that can be blended with other reducers for varied dry times.
|
|
RETARDER (RU315)
Designed for the Kosmic Urethane system to retard dry time in situations where this is deemed necessary. May be added to faster reducers to slow their dry time in emergency situations.
|
|
KRATOR ELIMINATOR (KE170)
KE170 is a fisheye additive that doesn't need to be used in every coat. It corrects fisheyes or crater defects, and works with lacquer, urethane, acrylic enamel, acrylic urethane, polyurethane, etc. a must have product for your paint shop.
|
|
CATALYST (KU100)
This product is for use only with Kosmic Kandys and Kosmic Kolor Urethane Enamels. Must be mixed with UK or UB before use. |
|
EXEMPT CATALYST (KU150)
This product must be mixed with other products before use. KU150 is a multi-purpose catalyst for urethane finishes. It is used in the KO-SEAL® II Primer Selaers, UC35, and UFC35 Kosmic Klears. |
|
SLOW EXEMPT CATALYST (KU151)
This product must be mixed with other products before use. KU151 is a multi-purpose catalyst for urethane finishes. It is used in the KO-SEAL® II Primer Selaers, UC35, and UFC35 Kosmic Klears. Replaces KU500. |
|
CATALYST (KU190)
For use in UFC19 Komply Klear® only and must be mixed with UFC19 before use. |
|
CATALYST (KU200)
Use with striping and lettering urethanes only. |
|
|
|