IRIDESCENT YELLOW CHROMATE
After preparing the part to accept the process, the part is simply dipped into a solution for a few minutes. The zinc & the chromate react to form the new colors. To improve those older zinc (pot metal) castings, plate with a fresh zinc plate before chromating.
The Yellow Chromate is a yellow/bronze iridescent finish on plated cadmium and zinc. Liquid concentrate is used at 0.5% to 3% by volume in water at 65° to 90°F. The finish has outstanding resistance to salt spray, greatly surpasses the normal 96 hour salt spray resistance specified for yellow chromates on zinc. It will withstand up to 200 hours salt spray. The deposit is a pleasing finish in itself. It is an excellent base for paint. The finish may be dyed to various colors.
4 fl oz bottle - makes 4 gallons
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.
![]() |
![]() |
![]() |
![]() |
Product Tags
Use spaces to separate tags. Use single quotes (') for phrases.
Check items to add to the cart or select all
-
-
Anodizing Products (69)
-
Anodizing Kits (3)
-
Anodizing Dyes (53)
-
-
Chrome Plating Kits (54)
-
Nickel Plating Kits (57)
-
Copper Plating Kits (45)
-
Gold Plating Kits (19)
-
Gold Tank Plating (10)
-
Gold Brush Plating (18)
-
-
Silver Plating Kits (13)
-
-
Chromates (5)
-
-
Tin Plating Kits (11)
-
-
Metal Strippers (11)
-
Books and Videos (6)
-
-
Plating Crystals (13)
-
Other Chemicals (47)
-
Anodes (15)
-
-
-
Plug N' Plate® Kits (27)
-
-
-
-
Black Oxide Kits (17)
-
Antiquing Solutions (14)
-
-
Buffing/Polishing (437)
-
Buffing Wheels (80)
-
Sisal Wheels (6)
-
Razor Buffs (3)
-
Scrubber Wheels (2)
-
Sisal Rope Buffs (1)
-
Mushroom Buffs (4)
-
Facer Buffs (3)
-
Cushion Buffs (3)
-
Tapered Buff (1)
-
String Buff (1)
-
Hourglass Buff (1)
-
Felt Wheels (5)
-
Liquid Polishes (4)
-
Wheel Rake (2)
-
Buffing Machines (15)
-
Buffing Adapters (20)
-
Shaft Extenders (10)
-
Bench Mandrels (2)
-
-
Buffing Kits (24)
-
Sanding Supplies (5)
-
Wet/Dry Sandpaper (14)
-
Abrasive Wheels (28)
-
Flap Wheels (9)
-
-
Cartridge Rolls (8)
-
-
Felt Bobs (17)
-
Diamondite® (22)
-
Waxes & Polishes (53)
-
Peek Polish (4)
-
ShineSeal (2)
-
-
-
Powder Coating (187)
-
Powder Coating Colors (106)
-
Metallic Coatings (11)
-
Candy Top Coats (16)
-
Powder Coating Ovens (11)
-
Curing Lamps (3)
-
-
Starter Kits (2)
-
-
Masking Products (11)
-
Primers (7)
-
-
Restoration Aids (309)
-
Permatex® Products (103)
-
Permatex® Cleaners (10)
-
Permatex® Sealants (11)
-
-
Evercoat Products (19)
-
Glyptal (3)
-
Metal Etching (2)
-
Tech-Line Coatings (25)
-
Lab Metal® (7)
-
Plasti Dip (45)
-
Welding Products (7)
-
Repair Pastes (5)
-
-
Cyclone Abrasives (23)
-
-
Paints and Coatings (515)
-
VHT Aerosol Paints (99)
-
VHT Motor Brite (1)
-
VHT Quick Coat (13)
-
VHT Epoxy Paint (3)
-
VHT Strip Fast (1)
-
VHT Primecoat (6)
-
VHT Vinyl Dye (7)
-
VHT Night Shades (1)
-
-
Krylon Fusion (40)
-
Krylon Engine Paint (12)
-
-
-
Camouflage (45)
-
Skull Patterns (8)
-
Metal Patterns (8)
-
Animal Patterns (9)
-
Marble & Stone (4)
-
Illusion Patterns (15)
-
Accessories (6)
-
-
Plasti Dip (47)
-
Plasti Dip Spray (24)
-
-
-
-
Gun Metal Bluing (3)
-
DuraCoat (4)
-
Shake N' Spray Kits (13)
-
Shake N' Bake Kits (10)
-
CamoPack Plus (11)
-
-
You have no items to compare.
You have no items in your shopping cart.
-
Having problem/questions about my cc power suppley
05.22.2013 19:05
So this is what I'm currently using DC Power Supply - Plating and Anodizing...
-
Powder over chromed part?????
05.21.2013 21:05
I've tried shooting candy colors over chrome, but haven't had much luck...
-
Cathode to Anode ratio
05.20.2013 15:05
I’ve read that you should have at least a ratio of 1:1 cathode to anode for...
-
Buying a gun, which do you recommend? Ez50 or hyper smooth 2.0 ?
05.19.2013 15:05
Bought a wai/craftsman style but sent it back, felt like it was gonna break...
-
Various Tank Liquid Levels
05.18.2013 16:05
Folks, I was wondering if the is some kind of “rule of thumb” for the amount...
- Glass, Ceramic or Titanium Heater - aquarium heaters work well
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.