Includes a 1.5 Gal Nickel Plating Kit and a 1.5 Gal Acid Copper Plating Kit.
Useful to put a heavy layer of copper plating over non-ferrous metals (copper, brass, bronze, zincated aluminum), then polish and nickel plate.
1.5 Gallon Kit Contains:- 3 x 2 Gal Plating Tanks & Lid
- 2 x 6" x 8" Nickel Anodes and Bandages
- 1 Pack Nickel Crystals with Brightener (Makes 1.5 Gals)
- 2 x Copper Anodes 4" x 8" and bandages
- 1 Pack Copper Crystals (Makes 1.5 Gals)
- 1 x 1.5oz Copper Brightener A
- 1 x 4oz Copper Brightener B
- 1 Pack SP Degreaser (Makes 4 Gals)
- 1 x 200W Glass Heater (for copper)
- 2 x Pump Filter/Agitators
- The Caswell Plating Manual
- Free Technical Support
Product Tags
Use spaces to separate tags. Use single quotes (') for phrases.
Check items to add to the cart or select all
-
-
Anodizing Products (69)
-
Anodizing Kits (3)
-
Anodizing Dyes (53)
-
-
Chrome Plating Kits (54)
-
Nickel Plating Kits (57)
-
Copper Plating Kits (45)
-
Gold Plating Kits (19)
-
Gold Tank Plating (10)
-
Gold Brush Plating (18)
-
-
Silver Plating Kits (13)
-
-
Chromates (5)
-
-
Tin Plating Kits (11)
-
-
Metal Strippers (11)
-
Books and Videos (6)
-
-
Plating Crystals (13)
-
Other Chemicals (47)
-
Anodes (15)
-
-
-
Plug N' Plate® Kits (27)
-
-
-
-
Black Oxide Kits (17)
-
Antiquing Solutions (14)
-
-
Buffing/Polishing (432)
-
Buffing Wheels (80)
-
Sisal Wheels (6)
-
Razor Buffs (3)
-
Scrubber Wheels (2)
-
Sisal Rope Buffs (1)
-
Mushroom Buffs (4)
-
Facer Buffs (3)
-
Cushion Buffs (3)
-
Tapered Buff (1)
-
String Buff (1)
-
Hourglass Buff (1)
-
Felt Wheels (5)
-
Liquid Polishes (4)
-
Wheel Rake (2)
-
Buffing Machines (15)
-
Buffing Adapters (20)
-
Shaft Extenders (10)
-
Bench Mandrels (2)
-
-
Buffing Kits (24)
-
Sanding Supplies (5)
-
Wet/Dry Sandpaper (14)
-
Abrasive Wheels (28)
-
Flap Wheels (9)
-
-
Cartridge Rolls (8)
-
-
Felt Bobs (17)
-
Diamondite® (22)
-
Waxes & Polishes (53)
-
Peek Polish (4)
-
ShineSeal (2)
-
-
-
Powder Coating (185)
-
Powder Coating Colors (104)
-
Metallic Coatings (11)
-
Candy Top Coats (16)
-
Powder Coating Ovens (11)
-
Curing Lamps (3)
-
-
Starter Kits (2)
-
-
Masking Products (11)
-
Primers (7)
-
-
Restoration Aids (309)
-
Permatex® Products (103)
-
Permatex® Cleaners (10)
-
Permatex® Sealants (11)
-
-
Evercoat Products (19)
-
Glyptal (3)
-
Metal Etching (2)
-
Tech-Line Coatings (25)
-
Lab Metal® (7)
-
Plasti Dip (45)
-
Welding Products (7)
-
Repair Pastes (5)
-
-
Cyclone Abrasives (23)
-
-
Paints and Coatings (513)
-
VHT Aerosol Paints (99)
-
VHT Motor Brite (1)
-
VHT Quick Coat (13)
-
VHT Epoxy Paint (3)
-
VHT Strip Fast (1)
-
VHT Primecoat (6)
-
VHT Vinyl Dye (7)
-
VHT Night Shades (1)
-
-
Krylon Fusion (40)
-
Krylon Engine Paint (12)
-
-
-
Camouflage (45)
-
Skull Patterns (7)
-
Metal Patterns (8)
-
Animal Patterns (9)
-
Marble & Stone (4)
-
Illusion Patterns (15)
-
Accessories (6)
-
-
Plasti Dip (47)
-
Plasti Dip Spray (24)
-
-
-
-
Gun Metal Bluing (3)
-
DuraCoat (4)
-
Shake N' Spray Kits (13)
-
Shake N' Bake Kits (10)
-
CamoPack Plus (11)
-
-
You have no items to compare.
You have no items in your shopping cart.
-
Silver plating coper ,76 mesh
05.23.2013 15:05
Dear fellow humans, I am so please I have found this forum. I have .5mm...
-
Having problem/questions about my cc power suppley
05.22.2013 19:05
So this is what I'm currently using DC Power Supply - Plating and Anodizing...
-
Powder over chromed part?????
05.21.2013 21:05
I've tried shooting candy colors over chrome, but haven't had much luck...
-
Cathode to Anode ratio
05.20.2013 15:05
I’ve read that you should have at least a ratio of 1:1 cathode to anode for...
-
Buying a gun, which do you recommend? Ez50 or hyper smooth 2.0 ?
05.19.2013 15:05
Bought a wai/craftsman style but sent it back, felt like it was gonna break...
- Glass, Ceramic or Titanium Heater - aquarium heaters work well
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.