Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > Buffing Supplies > Specialized Buffing Compounds
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Specialized Buffing Compounds

 

 

FAST CUT GREASY TRIPOLI COMPOUND

This is a greasy, extra fast cutting grade of Tripoli containing a high percentage of aggressive abrasives combined with Tripoli Powder, which produces a faster
cutting action. Used extensively on heavy buffing work and all types of automatic buffing machines.

2" X 2" X 10" Bar

Applications Of This Product
  • A wide variety of products for specialized metal finishing uses.

Related Products

 

Quantity Product Code Name Grade Price  
F515-6105 Fast Cut Greasy Tripoli Compound T-12 $9.99
Not Hazardous
F515-6105C Fast Cut Greasy Tripoli Compound x 6 T-12 $54.99
Not Hazardous

ROUGE FOR HARD CHROME PLATE

ROUGE FOR HARD CHROME PLATE

Developed especially for buffing down hard chrome plated surfaces to a smooth lustrous finish. Cuts fast and leaves the work clean.

2" x 2" x 10" Bar

Quantity Product Code Name Grit Price  
F515-6112 Rouge for Hard Chrome Plate C-25 $13.99
Not Hazardous
F515-6112C Rouge for Hard Chrome Plate x 6 C-25 $77.99
Not Hazardous

BLACK MAGIC ROUGE (Medium Greasy High Luster)

BLACK MAGIC ROUGE


A favorite for finishing brass, aluminum, copper, tin plate and other alloys. Will bring out a mirror-like luster on the work. Being a medium greasy grade it is ideal for the all around buffing job, requiring a brilliant finish.

2" x 2" x 10" Bar

Quantity Product Code Name Grade Price  
F515-6115 Black Magic Rouge Grade A $13.99
Not Hazardous
F515-6115C Black Magic Rouge x 6 Grade A $77.99
Not Hazardous

GREEN ROUGE

GREEN ROUGE

A very dry compound made with green chromium oxide powder. Used in the jewelry trade for extremely fine color buffing jobs on all classes of metals. Also used for buffing
precision tools, dies, and plug gages to a mirror bright finish and to remove light "metal fuzz" or lap lines with out disturbing the essential dimensions of the work.

1.5" x 1.5" x 7" Bar

Quantity Product Code Name Grade Price  
F515-6124 Green Rouge J-52 $11.99
Not Hazardous
F515-6124C Green Rouge x 6 J-52 $64.99
Not Hazardous

ALUMINUM BUFFING WHEEL BAR COMPOUNDS

CUT & COLOR - GRADE A-14

This grade was developed to "cut down" and "color" aluminum in one buffing operation on hand and automatic buffing machines. Brings up a high luster, leaving the buffed work clean and free of excess grease, or dirt.

2" X 2" X 10" Bar

Quantity Product Code Name Grade Price  
F515-6126 Aluminum Cut & Coloring Compound A-14 $11.99
Not Hazardous
F515-6126C Aluminum Cut & Coloring Compound x 6 A-14 $64.99
Not Hazardous

HIGH LUSTRE - GRADE A-15

A very dry grade intended for buffing small work to a high luster. Will not pack into
small cavities or recesses. If a brighter finish than No. A-14 Compound is desired,
re-buff using A-15.

2" X 2" X 10" Bar

Quantity Product Code Name Grade Price  
F515-6127 Aluminum High Lustre Compound A-15 $11.99
Not Hazardous
F515-6127C Aluminum High Lustre Compound x 6 A-15 $64.99
Not Hazardous

NON-FERROUS COLORING BAR COMPOUNDS
SOMETIMES REFERRED TO AS WHITE OR BLACK DIAMOND BUFFING COMPOUND.

Intended for buffing non-ferrous metals where the work surface is in good condition, free of deep tool or die marks. When heavy marks are present, Tripoli Buffing Compound is generally used to first cut down the surface and then a second buffing operation is performed using a "Coloring" Compound to produce a mirror-bright finish.

COLORING COMPOUND (MEDIUM GREASY)

COLORING COMPOUND (MEDIUM GREASY)

Our most popular grade because it is adaptable for cutting down and coloring the average run of aluminum, brass, and die cast metals. Also used extensively for buffing copper plated articles, particularly where a regular Tripoli Compound is too
severe and removes too much of the copper-plate. Contains a sufficient amount of grease binders to be used on most automatic buffing applications.

Quantity Product Code Name Grade Price  
F515-6133 Coloring Compound (Med Greasy) D-35 $9.99
Not Hazardous
F515-6133C Coloring Compound (Med Greasy) x 6 D-35 $54.99
Not Hazardous

HIGH COLOR COMPOUND (EXTRA DRY)

HIGH COLOR COMPOUND (EXTRA DRY)

An extra dry grade developed for "coloring out" operations on brass and sheet aluminum. Its light cutting action minimizes the danger of cutting too aggressively on the metal. Also recommended on recessed or indented surfaces that ordinarily would pack up with a greasier grade, giving difficult cleaning
problems. Leaves a clear bright finish, free of dirt.

Quantity Product Code Name Grade Price  
F515-6134 High Color Compound (Extra Dry) D-38 $9.99
Not Hazardous
F515-6134C High Color Compound (Extra Dry) x 6 D-38 $54.99
Not Hazardous
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
   
Login or Email
Password
Lost Password?
Create An Account