Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > Buffing Supplies > Introduction To Buffing and Polishing
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Ask Buffing Questions on our Buffing Forum

View Pictures Of Parts Polished With Our Products

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Introduction To Buffing And Polishing

 

AN INTRODUCTION TO BUFFING & POLISHING

All Products On This Page Can Be Purchased From Us Here

Ask Metal Polishing Questions On Our Forum

Download & Print The Complete Booklet - 730 KB Get Adobe Acrobat

Buffing and polishing using wheels and 'compounds' is somewhat like using wet and dry sanding paper, only much faster. Instead of using 'elbow grease' you will be using the power and speed of an electric motor.

The edge, or face, of the wheel is the 'sanding block', which carries a thin layer of 'compound' which is the sandpaper. Varying types of wheel are available, and the different grades of compound are scaled similar to sandpaper. The compounds are made from a wax substance which has the different abrasive powders added to it. When this hard block is applied to the edge of a spinning buffing wheel, the heat from the friction melts the wax, and both wax and abrasive are applied in a thin slick to the face of the wheel.

The objective of buffing and polishing is to make a rough surface into a smooth one and, of course, each work piece will be in a different condition, so will need different procedures. Imagine the surface magnified thousands of times, it will look like jagged mountains and valleys. By repeated abrasion, you are going to wear down those mountains until they are old, soft, rolling hills! Then they will not dissipate the light, but reflect it. It is the reflection that makes the buffed part appear shiny.

Reflected Light

TRICKS OF THE TRADE

Repairing small dents

Sand the inside of the part with emery paper. This will show you exactly where the dent is. Using a piece of end grain wood as a block, gently beat out the dent with a hammer.

Clean your buffing wheels with a WHEEL RAKE

Wheel Rake

Offer the jagged blade to the edge of the spinning wheel, and work it across the face until the wheel looks bright and fluffy once more. This action, done periodically, will remove entrapped metal particles, which could scratch a more delicate part.

Eliminating 'Swirl' Marks

Swirl marks caused by buffing in the final stages can easily be removed by wetting the part with a damp cloth, then dusting with a powder such as:- Whiting, Talcum Powder or Corn Starch, then buff on your wheel again until the swirls disappear.

One Wheel For One Compound

Applying different compounds to the same wheel only causes problems, because you end up with a mixture of abrasive surfaces, and metal deposits left over from the more abrasive operation. These microscopic particles only scratch the surface, destroying any benefit gained by the finer compound. To remove excess compound from the work, apply a small amount of talc to the work and the wheel, then rebuff.

Applying Compound

LITTLE & OFTEN is the rule. Too much compound will reduce the effectiveness of the cutting action, because the surface will become TOO greasy and over lubricated. This can often be seen by the prescence of a black slick of compound that seems to reveal around the work piece. Apply compound to the wheel for approx 1 second. Any more is wasted.

CHOOSING THE RIGHT WHEEL

There are different types of wheels and these have different effects on the compound they are used with. For example, the SISAL wheel is a coarse 'rope like' fiber, which frays out to make a sort of brush. These fibers have a very beneficial effect on scratched and rougher surfaces, almost stroking them smooth. When used with a course 'EMERY' compound, they 'cut' the metal down very rapidly. You could use this compound on a SPIRAL SEWN wheel and it would work, but the job would take much longer because the softer SPIRAL SEWN wheel is not going to thrash the metal so aggressively.

As you progress through the buffing compounds, you will change your buffing wheel, ending up using a soft polishing wheel,such as the CANTON FLANNEL with the least abrasive BLUE or RED compound which only polishes, it has no cutting action.

So, depending on the job in hand, you will determine which abrasive compound and wheel you are going to use first, then step down through the stages until YOU are satisfied with the results. Compounds are made from a mixture of fine abrasive fillers and a sort of greasy wax. The compound is melted, by friction heat, as the bar is pressed to the revolving wheel. This applies a thin layer of abrasive, 'glued' onto the cloth wheel, making it similar to an emery paper, only much faster!

Do not apply the compound after the workpiece, or on its own. This wastes material and is much less efficient.

By applying the material before the workpiece, you actually use the workpiece to force the compound into the buff. This is much less wasteful, more efficient and will actually speed up your buffing times.

Maximum Thickness Of Wheels

Motor Size

Wheel Diameter

 

4”

6”

8”

10”

12”

1/6 hp

1”

5”

-

-

-

1/4 hp

1.5”

1”

5”

-

-

1/3 hp

2.5”

2”

1”

-

-

1/2 hp

3”

2.5”

2”

1”

-

3/4 hp

4.5”

3.5”

2.5”

2”

1”

2 hp

4.5”

4.5”

4.5”

3”

1.5”

The table above show the THICKNESS of wheels. You may use multiple wheels to make up total permissible width.

CUT AND POLISH MOTIONS

There are two basic buffing motions you should use.

1. CUT MOTION gives you:- SMOOTH SURFACE, SEMI-BRIGHT & UNIFORM.
The workpiece should be moved AGAINST the direction of the wheel, using a MEDIUM to HARD pressure.
Cut Motion
2. COLOR MOTION gives you:- BRIGHT, SHINY & CLEAN SURFACE. The workpiece should be moved TOWARD the direction of the wheel, using a MEDIUM to LIGHT pressure. Color Motion

BUFFING SPEED AND PRESSURE

The correct pressure must be applied to the workpiece to provide the best finish economically and safely. Inadequate pressure will give NO buffing action.

Excessive pressure will cause the buffing wheel to slow down or actually collapse. This can also result in burn marks on the workpiece.

BUFF RUNNING SPEEDS

For best results your wheel should maintain a surface speed of between 3600 & 7500 Surface Feet Per Minute. (SFPM). The higher your speed, the better and quicker your results.

Formula for calculating surface speed of wheel in SFPM.
SFPM = 1/4 x diameter of Wheel x RPM (revs of spindle per min.)

Buffing Speeds

Therefore an 8” wheel @ 3600 RPM =2 x 3600 = 7200SFPM. Spindle speeds can be increased by a step pulley on a motor shaft.

For the workshop where only the occasional piece of work needs to be buffed, an economic alternative to purchasing a special machine is to simply adapt a bench grinder. Whilst this does not have the extended shaft, it can still do a formidable job.

All the guards need to be taken off and the grinder mounted on the edge of a workbench. This will allow access to the wheel from many angles. Alternatively, a small used washing machine motor can be used. With access to a lathe, a simple pointed taper can be made to fit over the shaft. Then the buffing wheels can be aimed on to the point. On smaller pieces, an electric drill with one of our shank mounted buffs will do an excellent job. Of course, if you want a pre-made, ready to use system, we sell an excellent range of buffing machines.

Buffing Machine
Caswell 3/4HP Buffer
Available in 1100RPM and 3450RPM

Some of our customers have even placed a large hand grinder in a vice, then changed the grinding wheel for a buff. These machines usually have very high speeds with good power, so they should be considered as another option.

Whenever you are making up something to do a buffing job, your prime consideration should be your safety.

If the buff pulls the piece from your hands, you should consider where it is likely to go. Remember it will be traveling at a fair speed, so no one should be in its way!

Is the machine mounted safely? It will have to stand a fair amount of abuse, so make sure it is WELL fastened down.

DISCLAIMER - Buffing machines can be dangerous. We accept no liability for their use/misuse or for accidents caused by the removal of guards.

SAFETY FIRST

There are two distinct areas on a buffing wheel -

THE UNSAFE AREA which is rotating towards the workpiece.

THE SAFE AREA which is rotating away from the workpiece.

Safe & Unsafe Areas

The division of these two areas is marked with the dotted line on the above drawings. The workpiece must only be applied to the area of the buff that is rotating AWAY from the workpiece.

You should ensure that you are completely aware which area is which, otherwise you could have a serious accident. Objects being thrown away from a buffing wheel can be traveling at very high speeds, which can result in some very unpleasant and potentially deadly accidents!

When buffing parts have sharp corners, edges or hooks, they should be offered to the wheel with the edge flowing away from the buff, so the part does not catch. Operators should ALWAYS wear SAFETY GOGGLES, APRON, GLOVES and DUST MASK.

DETERMINING GRIT SIZES of SANDPAPERS and BUFFING COMPOUNDS

We often get asked, 'Which grit should I use first?” Unfortunately, there is no cut and dried answer to this, because it really depends on the condition of the part. So, lets discuss some examples:

1) Aluminum Side Cover with one deep scratch.

To successfully remove the scratch, ALL of the material around the scratch has to be disposed of. In our example, this means a lot of aluminum! Initially, we are concerned with getting as much aluminum sanded off as quickly as possible, so we would use the coarsest abrasive available, say a 40 grit sandpaper on a flat block. It would be of NO USE to try to buff out this deep scratch with a buffing wheel, because the wheel would remove more material from the hole, as well as the surrounding areas. By keeping the abrasive on a flat block, no further material can be removed from the hole.

As the scratch is lessened, the grit size of paper is reduced from 40, to 80, 120, 240, 320 and finally 600. Once the surrounding material is removed, then the actual polishing can be started.

Buffing compounds will be determined by the size of the scratches. If you have used a 600 grit paper, you may like to proceed directly to a white buffing compound. If fine scratches are visible, then you'll need to 'back off' and go to the black compound before retrying the white.

2. Aluminum Side Cover - just dull.

Obviously, it would be a step backwards to start treating this piece by using the technique in our first example. As there is no large metal content to be removed, you could virtually dispense with the sandpapers and move directly to the polishing aspect of the part. The Brown buffing compound with a spiral sewn wheel could be employed to see if the shine is good enough. If not, then use a black compound, and then rework the part using the brown compound.

3. Aluminum Wheel Casting.

Many wheels are prepainted, directly over a rough sand casting. Remove the paint using VHT Stripfast, to expose the aluminum. The 'pimples' caused by the sand cast have to be removed to flatten the metal ready for polishing. Because of the difficult contours of the wheel, it is virtually impossible to sand with a flat block, so this is where Greaseless Compound comes in. Start off with the 80 grit, using a spiral sewn wheel or, for the awkward areas, a felt bob. Then proceed through the various grit sizes of Greaseless, until the metal is smooth , all 'pimples' are removed and an even 'flat' finish is achieved. The polishing should only begin once all traces of 'pimples' are gone. Use Black Compound for most of the polishing work, and finally, on a fresh or cleaned wheel, buff lightly with the Brown compound.

WHICH WHEEL & COMPOUND?

Use this chart to determine which wheels and compounds to use to polish different metals. This is a guide...experienced polishers will vary the materials used to suit the application and their technique. This chart serves as a good starting point for beginning polishers, but feel free to experiment.

Wheel & Compounds

BLACK = Emery Compound, a course abrasive material for removal of scratches, pits, paint,
rust etc.
BROWN = Tripoli compound used for general purpose cut and color on most soft metals.
WHITE = Blizzard compound, used for color and final finish of harder metals, has a cutting action.
RED = Jeweller’s Rouge, designed to polish without any cutting action. Safe on thin plates. Use
on its own wheel.
BLUE = A dryer, almost greaseless wheel - designed to polish without any cutting action. Safe
on thin plates. Use on its own wheel.
GREEN = Used exclusively for Stainless Steel.

THE THREE BUFFING STAGES
A = Rough Cut To Remove Scratches
B = Final Cut & Initial Polish - At Stage B, you should first use your wheel with a cutting action, then finish with a color action.
C = Final Polish (or luster)

Common Buffing Wheels

Sisal Wheel

THE SISAL BUFFING WHEEL

Sisal is a slender, hard, cellular strand of fiber that has demonstrated its great strength and tough resiliency in the form of binder twine, cord & rope for many years. These qualities, along with its natural abrading and grease absorbing characteristics, provide an ideal buffing wheel fabric.

Sisal buffing wheels will provide both polishing and cutting action. They will remove stretcher strains, orange peel, polishing wheel grit lines, light die marks, etc. To effect a fast cut, use a sisal wheel with the Black Emery compound or any of the greaseless compounds.

Spiral Sewn Cotton Wheel

THE SPIRAL SEWN WHEEL

Spiral sewn wheels are the workhorse of most buffing and polishing jobs. Because the plies of cotton cloth are sewn together spirally, the wheel becomes much harder and more pressure can be exerted on it. This is especially useful when ‘cutting’ the metal. The faces of these
wheels are pre-raked to accept compound immediately.

Loose Cotton Wheel

THE LOOSE COTTON WHEEL

The main purpose of a loose cotton wheel is to polish and cut in a similar manner to the Spiral sewn wheel, except that this wheel, not being tightly stitched together, will ‘mush’ or collapse, allowing the
cotton to get into awkward places more easily. If you have an object with fine details and awkward crevices, then this is the wheel to use.

Canton Flannel

THE CANTON FLANNEL WHEEL

Canton Flannel is a very soft material, and therefore is ideal for polishing items where a gentle touch is needed. Canton Flannel wheels are used in the jewelry trade to polish items with gold or silver plating, where no removal of metal is desired. They can also be used to polish plastic and lacquered items such as guitars.

Domet Flannel

DOMET FLANNEL WHEEL

Domet Flannel is the softest buffing material available. It can be used in any situation where an extremely soft touch is required.

Denim Buffs

DENIM BUFFING WHEELS

Our newest buffing wheel, the denim buffing wheel, is soft enough for any buffing application that calls for cotton wheels, but, because of the sturdy denim construction, it lasts much, much longer than a cotton buff. The faces of these wheels are pre-raked to accept
compound immediately. Use With Any Compound

Treated Spiral Sewn Wheel

TREATED SPIRAL SEWN WHEELS

These buffs are specially treated to give longer life than standard buffs. This treatment makes them much harder than regular cotton buffs, which allows the user to exert more pressure onto the wheel and gets the job done faster. Use with any compound just like
standard spiral sewn wheels.

Cushion Buff

CUSHION BUFFS

These buffs are sewn with two rows to slightly stiffen the buff.This improves the speed of the final coloring operation, giving you performance somewhere between a spiral sewn and a loose wheel.

Treated Vented Buffs

TREATED VENTED BUFFS

These buffs are specially treated to give longer life than standard buffs. They cut and color faster and are vented to keep the workpiece cooler. Hard center allows fast mounting to tapered spindle for quick change. Use with any compound.

Untreated Vented

UNTREATED VENTED BUFFS

The folded pleats hold more compound and keep the part cooler, resulting in a being twice as fast as a Spiral Sewn wheel. 10” wheels require 3” washers. These wheels are softer than their yellow cousins.

String Buff

STRING BUFF

Thousands of thin cotton string strands will buff all types of plastics, including bacolite, to a shiny surface. The buff is specially designed to keep the plastic cool. Bring side markers, turn signals, tail light lenses to shiny, like new condition. Thousands of 1-3/4” long cotton strands reach deep into details to gently polish and shine without overheating and melting plastic. Use in conjunction with our Plastic Glo Compound.

Finger Buffs

THE FINGER BUFF

An aggressive wheel, designed to buff irregular contoured metals, especially useful for buffing of checker plate. The treated sewn cloth fingers penetrate into crevices etc. and at the same time reduce friction eat buildup, so reduces the possibility of distorting thin metal panels etc. Use with Greaseless or black emery compounds. The wheel comes with a 5/8” hole in the metal center. ½” inserts are available.
Fits the Makita type Buffer/Polishers for ultra fast buffing of large surface areas, such as RV’s, boats, trailers, trucks, etc.

Sisal Rope Buff

SISAL ROPE BUFF

With a thickness of 2”, this long lasting wheel is an economic alternative to stacking sisal wheels on a shaft. The fibers are treated and stiff, giving an excellent hard surface for the initial cut to de-burr etc. Use with Greaseless compounds or Black Emery

Mushroom Buff

MUSHROOM BUFF

Diameters are 2.5, 3.5 & 4.5 inches.
Ideal for buffing contoured shapes such as wheels. Use with any compound on a drill or flexible shaft.

Facer Buff

FACER BUFF

Diameters are 2.5, 3.5 & 4.5 inches.
Ideal for buffing the flatter areas, especially wheels. Use with any compound. Good for using greaseless for removing cast casting marks in aluminum.

Tapered Buffing Wheel

Tapered Buff

The pointed end is ideal for buffing inside holes and crevices, like the lug nut holes in wheels. Made from soft cotton. Use with any compound.

Scrubbing Mushroom Buff

SCRUBBING MUSHROOM BUFFS

Ideal for buffing contoured shapes such as wheels. Scrubber wheels remove rust, scratches, minor blemishes, old paint, and plating. Use a light touch. No compound is required, as
the abrasive is already impregnated in the wheel. Gives metal a "satin" appearance.

Flap Wheels

FLAP WHEELS

These tightly packed and bonded sheets of resin bonded aluminum oxide are great for sanding, shaping and polishing all types of materials. Especially good for removing paint and rust. Best
used on an electric drill or the Flexible Shaft.

Sanding Drums

SANDING DRUMS

Sanding drums are self expanding rubber spindles with hardened metal arbors and nuts. Precision manufactured to close tolerance, providing smooth and even performance. Use for: sanding, shaping,
grinding, finishing, polishing. Use on: wood, metal, plastic, fiberglass, rubber, glass or stone. Use with: portable drill or grinder, drill press, lather, flexible shaft, bench grinder. Especially useful for surfaces that are curved or irregularly shaped.

Nylon Bristle Brush

ABRASIVE NYLON WHEELS

Strands of nylon impregnated with a tough aluminum oxide abrasive. Removes old paint, rust, weld scale and burns. Cleans and polishes. Is ideal for wood because it cleans without gouging. It never loses its abrasive power, or its shape. Safe on
skin! Max 2500 rpm. Generally speaking, you will start off with a course abrasive
compound, then change to a medium compound and finally a fine compound, just as you would using sandpaper.

Hourglass Buff

HOURGLASS BUFF

We developed a special buffing wheel that fits straight into a drill chuck. The unique shape allows the buff to rest on the pipe without spinning off. By simply rotating the drill, all angles of the pipe can be buffed rapidly. The tapered end allows you to get into difficult corners. This buff is ideal for almost any tubing, such as handrails on boats, handlebars, tail pipes etc. Use with almost any buffing compound, but is especially useful with Blue Begone liquid polish.

There are lots more tips and tricks in our FREE Buffing Booklet. Download The Complete Booklet - 730 KB Get Adobe Acrobat