Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > > Restoration Gallery > Building A Motorized Tank Bar
Search Caswell Inc.

Web Site Features
Start Here

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Building A Motorized Tank Bar

 

A pictorial by one of our customers

Motorized tank bar in a zinc plating bath rotates @ 2rpm
Motorized tank bar in a zinc plating bath rotates @ 2rpm
Gives good even plating with little operator attention
Gives good even plating with little operator attention
Motor available at

Micro-Mark
340 Snyder Ave
Berleley Heights
NJ 07922

Trivet made of CPVC 1/2" diameter about 6" square drilled holes are to allow it to sink.
Trivet
1970 T120R Triumph Bonneville. All fasteners are zinc plated using the Caswell system.
All fasteners are zinc plated using the Caswell system
Trivet for tank bottom. Place aeration lines on top of this & it prevents sediment from being stirred up.
Trivet for tank bottom