Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > > Powder Coating Supplies >
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

What Are TGIC Powder Coatings?

 

Polyester TGIC coatings utilize the epoxy functional crosslinker TGIC (triglycidyl isocyanurate). Use of this low molecular weight, multifunctional crosslinker enables polyester TGIC formulations to contain 90% or greater resin within the binder system.  Weathering of polyester TGIC powders is comparable to polyester urethane coatings.

Polyester TGIC coatings typically offer faster or lower temperature curing than polyurethanes.  Unlike urethane coatings, TGIC's maintain excellent mechanical properties at film builds above 3 mils with no outgassing.  Additionally, TGIC coatings provide superior edge coverage when sharp edges are present.

Typical applications for polyester TGIC coatings include aluminum extrusions, automotive wheels, transformers, air conditioners, fencing, lawn and garden equipment, and gas cylinders.  

Pretreatment Iron phosphate, zinc phosphate Advantages: Excellent gloss retention
Application Conditions Electrostatic powder spray Excellent overbake color stability
40 - 100KV Good mechanical properties at high film build
Film Thickness 1.5 - 20.0 mils Good salt spray resistance
Specific Gravity 1.2 - 1.8 Wide range of colors
Coverage 107.0-160.0 sq. ft./lb. per mil of coating Releases minimal volatiles upon curing
Baking Schedules 5 minutes at 410° F Disadvantages: Difficult to get low gloss finish
(Standard Cure /  7 minutes at 399° F Difficult to get very smooth coating at low film build
Metal Temperature) 15 minutes at 375° F Less solvent resistant than urethane

TGIC Standard Cure Schedules

The data below is based on 20-gauge steel panels.  For heavier ware, higher temperatures or longer oven times may be necessary. Low Gloss or textured finishes may require a slightly longer cure.