Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
Login To Your Account
 
Home > > Plating, Anodizing and Metal Finishing > Pickle #4
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Ask Plating Questions On Our Forum

Online Plating Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Pickle #4

 

AT LAST! Eliminate using unpleasant muriatic acid.

For stripping rust from steel & also activates zinc, pot metal, lead, 60/40 solder, copper & its alloys.
No unpleasant fumes.

More moderate action, less pitting.

This system is ideal for the preparation of lead work such as bullets, sun catchers, lead came, etc.

Applications Of This Product
  • Strip rust
  • Activate Zinc, Pot Metal, Lead, Solder, Copper etc.
  • Prepare Lead for Plating

Related Products

Pickle #4 is a general-purpose metal activator and de-oxidizer containing fluoride. Used at room temperature on steel, copper, brass and zinc.

PICKLE #4 is a free flowing mixture of dry acids and is more convenient and safer to use than liquid mineral acids. It does not produce the undesirable fumes given off with strong acids. It is dissolved in water and used at ambient temperatures to remove light to medium surface rust from steel and to activate steel surfaces prior to blackening with Black Oxide blackening solutions. Heavily rusted surfaces may require elevated temperatures of 150°F to 170°F. No venting required when used at ambient temperatures. It is used following the water rinse after cleaning the steel surfaces with SP DEGREASER.

PICKLE #4 is more moderate in its action on steel surfaces than mineral acids and produces a uniformly active surface.

PICKLE #4 is also used to activate zinc-plated surfaces, die cast zinc surfaces, copper and copper alloy surfaces prior to blackening, oxidizing, antiquing, chromating or other finishing.

EQUIPMENT REQUIRED

PICKLE #4 solutions must be contained in acid-resistant tanks and containers. Polypropylene, polyethylene, PVC or rubber-lined steel are suitable. If heaters are required they must be glass or Teflon coated.

SOLUTION MAKE-UP

Metal Action Makeup & Use
Steel activation

8 oz/gallon
30 to 60 second immersion

  rust removal 16 to 32 oz/gallon
2 to 10 minutes immersion
Copper and its Alloys deoxidizing 8 to 16 oz/gallon
30 to 60 seconds immersion

Plated and die cast zinc
Lead/lead solder
deoxidizing 4 to 8 oz/gallon
30 seconds to 2 mins immersion

Residual PICKLE #4 solution must be removed with a thorough cold-water rinse prior to further finishing.

SOLUTION CONTROL

The strength of the solution is maintained by small periodic additions of PICKLE #4 salts. The solution is dumped only when its effectiveness is diminished by accumulation of metals, dirt, oil, etc.

Quantity Product Code Name Size Price  
PIC4 Pickle #4 2 lbs $15.96
No Air Shipping
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.