Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
Login To Your Account
 
Home > > Plating, Anodizing and Metal Finishing > Gold Tank Plating Kits
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Ask Plating Questions On Our Forum

Online Plating Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

24ct Gold Tank Plating Kits

 

CYANIDE FREE SYSTEMS

Gold Plating Watch

Work safely with cyanide free gold to plate jewelry, flatware, baby shoes, flowers, bathroom fittings and much more. 

Caswell 24ct Gold is ideal for immersion plating of larger items. For brush plating applications, please use our FastGold system.

Certainly, tank-plating gold requires much less supervision and effort than brush plating. 24Ct Gold plates @ 2 micro inches per minute using approx 3 volts. Plating time is 30-60 seconds, to provide a durable decorative finish.

An application of a VHT Clear Lacquer or Collinite Wax over a plated item will increase its wear, reduce water spotting and enhance the gold's color.

Cyanide free solution eliminates the dangers of deadly poisoning from ingestion through the skin or from the production of cyanide gas.

Applications Of This Product
  • Apply gold onto tin, copper, brass, bronze, nickel, silver, gold and most lead free solders.

Sample Work Completed With This Product

Gold Plated Clock

Toyota Emblem

Gold Plated Banjo

Telegraph Key


You Must Supply

Copper Pipe for tank bar

Copper Wire to hang items

Small amount of electrical wire to make connections

Power Supply


Related Products

1 Gallon Kit:

  • 1 x 300ma Power Supply (plates up to 20 sq")
  • 1 Gallon 24 ct Gold Solution
  • 1 x Tank Heater
  • 1 x 2 gal tank with lid
  • 2 x Stainless Steel Anodes
  • The Complete Plating Manual
  • Free Technical Support

2 Gallon Kit:

  • 1 x 300ma Power Supply (plates up to 20 sq ")
  • 2 Gallons 24 ct Gold Solution
  • 1 x Tank Heater
  • 1 x 3.5 gal tank with lid
  • 2 x Stainless Steel Anodes
  • The Complete Plating Manual
  • Free Technical Support

The system operates with either stainless steel anodes, or 24 carat gold anodes. Gold anodes prolong the life of the solution, but are obviously very expensive.

Caswell 24ct Gold will plate directly onto tin, copper, brass, bronze, nickel, silver and most lead free solders. Some alloys must be copper or nickel plated first. Steel must be nickel plated first.

Trying to match existing gold supplied by another company is difficult as shades may vary. (It is better to lightly recoat the old gold with a new layer)

The system contains 2 pennyweights gold per US Gallon of solution.

Plating Gold Onto Stainless Steel?

Eliminate nickel plating steps and plate gold directly onto stainless steel parts using our Stainless Steel Activator for Gold. Etch with this product, then plate gold directly onto stainless parts.

Prod SSAG1 - 1 Quart - $35.00

Quantity Product Code Name Size Price
GPS54 24 ct Gold Solution 1 pint $105.00
Not Hazardous
GPS85 24 ct Gold Solution 1 quart $189.00
Not Hazardous
GPS5215  24 ct Gold Solution 1 Gallon $656.00
Not Hazardous
GPS5395 24 ct Gold Solution 2 Gallons $1125.00
Not Hazardous
ANSTP1G Anodize & Chrome Stripper (concentrate) Makes 3 gal $44.94
No Air Shipping
ANSTP4OZ  Anodize & Chrome Stripper (ready for use) 8 oz $5.99
No Air Shipping
CAB10 Cabosil (gold gelling powder) 0.1 lb (Mix with 1 qt of gold) $12.99
Not Hazardous
GLDANOD24  24 ct Gold Anode 3/4" X 1" X 3/1000", 0.01 oz $109.00
Not Hazardous
SSANODE Stainless Steel Anode 4" x 8" $9.99
Not Hazardous
GLD250 24 ct Gold Tank Plating Kit

1 Gallon

$699.00
Not Hazardous
GLD415 24 ct Gold Tank Plating Kit

2 Gallon

$1199.00
Not Hazardous
SSAG1 Stainless Steel Activator For Gold 1 Quart $41.39
Not Hazardous
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
  * - Other minor household items may be required, such as gloves, water etc.