Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
Login To Your Account
 
Home > > Plating, Anodizing and Metal Finishing > Black Oxide Kit
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Ask Plating Questions On Our Forum

Online Plating Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Black Oxide Kit

 

Black Oxide Kit

This new technique was developed by the commercial gun blue manufacturers as a more environmentally friendly system than the commonly used hot application. Parts requiring blackening are simply placed in the liquid at room temperature, no electrical power is required.

Applications Of This Product

Sample Work Completed With This Product

Lathe Spindle

Firearm Bolt


You Must Supply

1 Metal Container for Sealing Step


 

Black Oxide Parts

Convenient - Easy to do in house. No waiting for heatup of blackening solution. No waiting for the unpredictable return of parts from an outside vendor. Eliminates high outside vendor costs. Retain control of production and quality. Ideal for high volume or short runs. Works especially well for blackening large volume of small parts in a rotating barrel.

Higher Productivity - Parts can be blackened in two minutes vs 15 to 30 minutes for hot oxide. Normally twice the amount of parts can be blackened in the same amount of time as with hot oxide.

Controllable - Long bath life, blackening solution may be replenished indefinitely with periodic additions of fresh concentrate.

So easy to install and use that you can now economically apply a pleasing decorative, sales-appealing black corrosion-resistant finish on parts previously left unfinished.

Versatility - Blackens cast iron, forged steels, mild steels, hardened tool steels and powdered metal parts. No white salt bleedout as is common with hot oxide.

Dimensional Control - No heat distortion. No smutty rub-off as with other room-temperature blackening processes.

Energy Cost Saving - Blackening is done at room temperature vs hot oxide blackening done at 290°F.

Safety - Blackening solution uses odorless, mild water-dilutable chemicals that require no venting vs hot oxide. No hazardous caustic chemicals with fumes that present health hazards and no spattering of hot, skin-burning chemicals.

Low Maintenance - Longer Equipment Life - No expensive pollution control equipment. 

Parts Coverage - 600 to 1200 sq. ft. of surface area blackened per gallon of concentrate.

How to achieve professional results in minutes:- Thoroughly clean the part to be blackened by either sandblasting, wire brushing, wire wool abrasive cleaning, or by scrubbing in 'VIM' or 'COMET' household abrasive cleaner. Make sure you have removed all rust, paint, oil and grease.

Immerse the part in the mixed Black Oxide Solution and swirl around for between 30 seconds and 5 minutes. Alternatively, the part may simply be placed in the solution for 5 - 10 minutes. Remove the part from the solution and rinse in fresh water.

Immediately brush on or dip into the Penetrating Sealant, and allow to soak in the liquid for 5-10 minutes. Shake off any excess and allow to dry thoroughly before handling. Penetrating Sealer imparts a slightly oily feeling to the parts. If a non-oily finish is desired, do not use the Penetrating Sealer after blackening, and instead use Caswell Sealer.

Black Oxide works on steel or iron parts only and will not blacken Stainless Steel - use Stainless Steel Blackener.

 

1.25 Gallon Kit:
  • 1 Pint Black Oxide Concentrate (makes 1.25 gal)
  • 2 x 1 Quart Penetrating Sealer
  • 1 x 2 Gal Plastic Blackening Tank
  • Instruction Sheet
  • Free Technical Support

2.5 Gallon Kit:

  • 2 x 1 Pint Black Oxide Concentrate (makes 2.5 gals)
  • 1 Gal Penetrating Sealer
  • 1 x 3.5 Gal Plastic Blackening Tank
  • Instruction Sheet
  • Free Technical Support

15 Gallon Kit:

  • 1 x 20 Gal Tank & Lid (12Wx24Lx18H)
  • 1 x 15 Gal Tank & Lid (12Wx24Lx12H)
  • 1.5 Gal Black Oxide Concentrate (Makes 15 Gal)
  • 10 Gal Penetrating Sealer
  • Instruction Sheet
  • Free Technical Support

45 Gallon Kit:

  • 5 Gallons Black Oxide Concentrate (makes 45 Gals)
  • 5 Gallons Penetrating Sealer
  • Instruction Sheet
  • Free Technical Support

Now Available - Black Oxiding Gel Kit

Easily spot blacken steel (not stainless) or iron. Simply apply the black oxide gel where you want the blackening to occur. The gel keeps the blackener in place. Leave it on the part for 1-3 minutes and rinse off. Seal with Caswell Sealer for a dry finish.

Black Oxide Gel Kit

Black Oxide Gel Kit Includes:

  1. 4 fl oz Black Oxide Concentrate Gel (covers approx 2 sq ft)
  2. 4 fl oz Caswell Sealer
  3. Disposable Vinyl Gloves

Caswell Sealer

Use Caswell Sealer instead of penetrating sealer to inhibit corrosion on blackened parts without imparting an oily feel. It is a clear, acrylic based lacquer. It is a mildly alkaline water based solution used to deposit a corrosion inhibiting hard, clear, glossy dry finish. It can be used on all bare metal surfaces and all types of conversion coatings, black oxide, antique/oxidized and phosphate finishes. It can be used at full strength or diluted with up to an equal volume of water. The coating is approx 0.09 mil thick and the solution covers approx 2900 sq ft per gallon. Dry time is 10 minutes at room temp.

Product can be applied by dipping, spraying or brushing.

For Stainless Steel:

Stainless Steel Blackener 370 is an acidic liquid concentrate used full strength or diluted with up to 3 parts water to blacken stainless steel at room temperature. Recommended for color coding parts and blackening engravings on stainless steels. Produces a pleasing dark gray/black finish. Seal with Caswell Sealer.

Now also available in a Gel formula kit. Blackener stays where you put it. Simply apply with a brush or swab, allow to sit on the part for 1-2 minutes and rinse off. Then seal with the included Caswell Sealer.

Stainless Steel Blackener Gel Kit

Stainless Steel Blackener Gel Kit Includes:

  • 4 fl oz Stainless Steel Blackener Gel (covers approx 2 sq ft)
  • 4 fl oz Caswell Sealer
  • Disposable Vinyl Gloves


Quantity Product Code Name Size Price  
BO1 Black Oxide Kit 1.25 Gal $44.99
No Air Shipping
BO2 Black Oxide Kit 2.5 Gal $79.99
No Air Shipping
BO15 Black Oxide Kit 15 Gal $799.00
No Air Shipping
BO3 Black Oxide Kit 45 Gal $699.00
Hazardous Goods
BOGK Black Oxide Gel Kit 4 fl oz $19.99
No Air Shipping
SEAL45 Caswell Sealer (non greasy) 1 Quart $54.99
Not Hazardous
SEAL1G Caswell Sealer (non greasy) 1 Gal $134.99
Not Hazardous
BOCONC1P Black Oxide Concentrate (1.25 Gal) 1 Pint $24.99
No Air Shipping
BOCONC1Q Black Oxide Concentrate (2.5 Gal) 1 Quart $39.99
No Air Shipping
BOCONC1G Black Oxide Concentrate (10 Gal) 1 Gal $129.00
No Air Shipping
BOCONC5G Black Oxide Concentrate (45 Gals) 5 Gallons $499.00
Hazardous Goods
PSEAL1P Penetrating Sealer 1 Pint $9.99
Not Hazardous
PSEAL1Q Penetrating Sealer 1 Quart $15.99
Not Hazardous
PSEAL1G Penetrating Sealer 1 Gal $54.00
Not Hazardous
PSEAL5G Penetrating Sealer 5 Gal $230.00
Not Hazardous
SSB370 Stainless Steel Blackener 370 (Not For Steel) 1 Pint $28.99
No Air Shipping
SSB3708 Stainless Steel Blackener 370 (Not For Steel) 8 fl oz $19.99
No Air Shipping
SSBGK Stainless Steel Blackener Gel Kit 4 fl oz $19.99
No Air Shipping
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
  * - Other minor household items may be required, such as gloves, water etc.