Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > > Buffing Supplies > Wood and Acrylic Polishing Kit
Search Caswell Inc.

Web Site Features
Start Here

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Wood and Acrylic Polishing Kit

 

Wood & Acrylic Buffing Kit

Applications Of This Product
  • Heavy Duty Buffing Machine for professional use.
  • Kit includes everything required to begin buffing.

Related Products

Low speed 1100RPM Buffing Machine is ideally suited for polishing wood, acrylic, lacquered surfaces, plastics and more. Perfect for guitar polishing!

Kit includes:

  • 1100RPM, 3/4 HP Buffing Machine
  • 6 x 12" diameter acrylic buffing wheels
  • 1 x Plastic Buffing Compound (Fine)
  • 1 x Plastic-Glo Buffing Compound (Ultra-Fine)
  • 5 each 120, 240, 400 and 600 grit Wet and Dry Paper
  • Wheel Rake
  • Instructions

Instructions:

If the object to be polished has heavy scratches, start by sanding. Start with 120 grit sandpaper, used dry. Switch to a 240 grit paper, dry. Finish with the 400 grit paper, used wet. Grits as fine as 600 may be used. Always use a wooden or rubber sanding block (not supplied). When removing scratches be sure to sand an area larger than the scratch. Sand with a circular motion, and use a light touch and plenty of water when using paper wet.

Polishing with the buffer will bring the surface a high lustre. Start with the Plastic Buffing Compound (Fine), and then switch to the Plastic-Glo Buffing Compound (Ultra-Fine). Be careful not to apply too much pressure, or excessive heat may cause burning of the part. Dedicate a buffing wheel for each compound, to avoid cross-contamination and introducing scratches into your final polish.

The buffing machine features large diameter, extended shafts, allowing easy access of larger parts. Heavy duty cast iron base and frame. Precision machined shaft and lubricated bearings for longer life. Single phase motor. May be mounted to a bench, or for greater access, to the optional stand.

  • 3/4 HP, 115V, 60 Hz, 7.8 amps
  • 1100 RPM
  • Spindle thread: 3/4'' x 12 TPI
  • Spindle length: 2-5/16''
  • Base: 8''L x 5-3/4''
  • Overall length of shaft - 30"
  • Height of shaft center from bottom of base - 6.5"
  • 12 month warranty

 


Buffing Stand
Buffing Machine Stand

Quantity Product Code Name Price  
WBC Wood and Acrylic Buffing Kit (Includes Machine) $279.00 $231.70
Not Hazardous
BUFF245 3/4 HP Buffing Machine - 1100 RPM (Machine Only) $236.50 $189.20
Not Hazardous
BS9945 Buffing Machine Stand $28.97
Not Hazardous
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
   
Login or Email
Password
Lost Password?
Create An Account