Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > > Repair Products > Epoxy Gas Tank Sealer
Search Caswell Inc.

Web Site Features
Start Here

Toll Free Order Line:
(855) CASWELL

Tech Support:
(315) 946-1213

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Epoxy Gas Tank Sealer

 

PHENOL NOVOLAC EPOXY GAS TANK SEALER

Save 20% On Our Motorcycle Kit By Liking Us On Facebook and buying the kit on Facebook.

1. Like Us on Facebook
2. Buy Kit on Facebook

Gas Tank Sealer

Applications Of This Product
  • Saves hundreds of dollars in repairs
  • Also works on plastic and fiberglass
  • Withstands modern ethanol fuels


Related Products

Permanently Repairs Steel, Aluminum, Fiberglass and Plastic Gas Tanks

Read The Application Instructions (24kb PDF)

Phenol Novolac Epoxies are a new breed of chemical resistant materials, able to withstand permanent immersion of many harsh solvents, fuels and oils. This Epoxy has much better bond strength than single component products, with strengths of up to 3000 PSI, and this higher strength reduces the need for a clinically clean surface, as the epoxy actually prefers to bond to a rough rusty surface. Our new phenol novolac is more thixotropic, which means it 'hangs' on the tank walls during the coating process. This gives a thicker overall coating. There is more volume of material in the kit to allow for this.

Gas Tank Sealer

What else can you use Gas Tank Sealer for?

  1. A corrosion and chemical resistant coating. ie: battery compartments.
  2. A high strength adhesive where plenty of working time is needed.
  3. A potting compound, to encapsulate electronics
  4. A non-skid surface, just bed in aluminum oxide.
  5. Relining old potato peeler machines (Hobart type) - coat liner and bed in aluminum oxide.
  6. Repair leaks in concrete vessels. Add fine sand to make a mortar.
  7. Bonds to almost anything except polyethylene (gas tanks are not made of polyethylene). Bonds to wood, plastic, rubber, concrete, metals.
  8. Making high quality molds - virtually no shrinkage on curing.
  9. Thin cross section repair of sheared parts, such as; broken cups, dishes, or a split leg on a chair.

Application Instructions

All traces of oil and gasoline should first be removed by pouring about 1 pint of acetone or lacquer thinner into the tank, and rotating the tank several times to thoroughly sluice the sides with solvent. Dispose of the contaminated solution.

When recoating your gas tank from failed Kreem or POR-15 tank sealers, remove the old, failed coating using a paint stripper containing Methylene Chloride.

Place a hand full of drywall screws into the tank and shake them around vigorously for several minutes. These will dislodge any loose particles of rust. In the case of Fiberglass and plastic tanks, this will rough up the tank interior, improving adhesion.

Rinse out the tank with about 1-pint of acetone or lacquer thinner, then set aside and allow to dry. Use an airline to blow air into the tank to aid drying.

Apply duct tape or masking tape to any weeping seams, holes or porous areas. This will stop any Gas Tank Sealer from oozing out, and will allow it to bridge over the hole. Plug the outlet ports with putty or Play-Doh. Mix up the required amount of Gas Tank Sealer (one unit should treat two small motorcycle tanks or one large one) If you are only treating ONE small tank, then divide parts A & B in half. You could use a dipstick to gauge this.

In a separate plastic container (margarine tub etc.) mix the two parts together thoroughly for at least 2 minutes. Scrape around the sides to ensure all resin is blended together. BAD MIXING AND BAD MEASURING IS THE #1 CAUSE OF FAILURE!!

Pour into the tank, then immediately seal up the filler hole with Gladwrap and an elastic band. Swill the tank around in every direction for several minutes to obtain a good layer of Gas Tank Sealer over all surfaces. Remove the filler cap,Gladwrap seal, and pour out any excess. Allow to drain upside down for a few minutes.
If you have a built in fuel filter, blow air into the fuel line port for about 10 minutes. This will clear the filter of any Gas Tank Sealer.

Scrape off any excess with a sharp knife at this point (usually about 40-60 Min after mixing) Place the tank in a warm 70-90 f place and allow to cure overnight. In the case of alcohol fuels, allow 3-5 days at room temperature, or 24 hours at 120 deg f.

Our Motorcycle Epoxy Gas Tank Sealer Kit coats two small motorcycle tanks or one large one.

A few weeks ago you sent me your gas tank sealer kit. In the meantime, I have tried it and I just wanted to tell you that IT'S A GREAT PRODUCT! It worked perfectly well! Now I have a perfect gas tank again for about 40 US$ (including spray paint etc.). A local repair shop wanted about 1000 bucks (no kidding!) for welding and repainting the tank . So, I guess I made a good deal. Thanks a lot for providing such a great product and also for your excellent service.

Best regards,

Aldo Hoermann

More Comments...

Bulk Reseller Pricing Available - Call 315-946-1213 To Place Orders

10 Kits - 20% Off
20 Kits - 25% Off
50+ Kits - 40% Off

Don't want to do it yourself? The following businesses use our Gas Tank Sealer to repair your tank.

 

Quantity Product Code Name Size Price  
GTS1750  Epoxy Gas Tank Sealer (Motorcycle Tanks - Up To 10 Gal) 1 Pint $39.99
No Air Shipping
GTSC Epoxy Gas Tank Sealer (Car Tanks - Up to 20 Gal) 1 Quart $69.99
No Air Shipping
GTS1G Epoxy Gas Tank Sealer (Tanks Up To 80 Gal) 1 Gallon $219.99
No Air Shipping
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
   
Login or Email
Password
Lost Password?
Create An Account